Before You Go, Let’s Talk About Your Parts
Tell us about your part, quantity, and key requirements. Nova Precision Manufacturing Co.,Ltd can help you choose suitable materials and manufacturing processes for your project.

Compare Type II and Type III anodizing for CNC aluminum parts, including thickness, wear, sealing, dimensional growth, masking, and RFQ details.
Type II anodizing is the general-purpose choice for aluminum CNC components that need corrosion protection, a cosmetic finish, or dyed color. Type III, also called hardcoat anodizing, is a thicker, denser oxide layer chosen mainly for wear, sliding contact, and abrasion. Both are electrolytic coatings defined in MIL-A-8625, and both grow partly into and partly out of the aluminum surface, so either one can push a precision feature out of tolerance.
For a buyer, the question is rarely “which type is better?” It is which type suits each surface of the part, how much dimensional change the design can absorb, and what the drawing must state so the machinist and the anodizer work to the same final size. This guide compares the two finishes on the points that affect cost, fit, and rejection risk, and ends with the information to put in an RFQ.
The core difference is function and thickness. Type II is conventional anodizing used for corrosion resistance, paint adhesion, and appearance. Type III is a heavy, dense coating specified when abrasion resistance is the main goal. Type III coatings are generally several times thicker than Type II, which is why they change dimensions more and leave less room for dyed color.
The MIL-PRF-8625F text reproduced by Anoplex gives typical thickness ranges of 0.00007 to 0.0010 inch for Type II and 0.0005 to 0.0045 inch for Type III. In metric terms, that is roughly 2–25 µm versus 13–114 µm. The ranges overlap at the thin end of Type III, but in practice the two types are specified very differently, as the table shows.
| Factor | Type II (conventional) | Type III (hardcoat) | What to confirm with the supplier |
|---|---|---|---|
| Primary purpose | Corrosion resistance, paint adhesion, appearance, dyeing | Abrasion and wear resistance | Which surfaces actually need each function |
| Typical thickness range (spec Table IV) | 0.00007–0.0010 in (about 2–25 µm) | 0.0005–0.0045 in (about 13–114 µm) | Required thickness stated on the drawing |
| Default thickness if none is stated | No default; Type II is controlled by minimum coating weight | 0.002 in nominal, with ±20% variation up to that thickness | Whether a thickness callout is needed for fits |
| Growth per coated surface | About half of coating thickness (design guidance) | About half of coating thickness (design guidance) | Processor’s measured growth on first articles |
| Sealing | Sealed unless otherwise specified | Left unsealed when maximum wear resistance is the goal; sealed only if specified | Sealed or unsealed, stated explicitly |
| Color | Wide dye range; the spec prefers Type II for dyed work | Mostly dark natural gray to black | Physical color sample for cosmetic parts |
| Alloy limits | Heat-treatable alloys in a heat-treated temper | Not for alloys above 5.0% copper or 8.0% silicon unless approved | Exact alloy and temper |
| Fatigue effect | Reduced; thicker coatings reduce it more | Reduced; usually greater because the coating is thicker | Whether the part is cyclically loaded |
Source basis: thickness, sealing, alloy limits, and fatigue statements come from the MIL-PRF-8625F text. The “color” and “purpose” rows are summarized from the same document and from supplier guidance.

Choose Type II when the part needs corrosion protection, a controlled cosmetic appearance, or a dyed color, and the coated surface will not carry significant sliding wear. Choose Type III when a surface will slide, rub, or be handled repeatedly. Decide surface by surface, because many parts need both.
Type III is the reference option for wear. The specification sets a wear-index limit for unsealed Type III coatings of 1.5 mg per 1,000 cycles for most alloys, and 3.5 mg per 1,000 cycles for alloys with 2% or more copper. One machine shop’s engineering comparison, True Precision Machining’s Type II vs Type III guide, publishes typical hardness of 200–400 HV for Type II and 400–600 HV for Type III against roughly 107 HV for 6061-T6. Those are one vendor’s typical values, not guaranteed properties. Treat hardness as a reason to ask for wear data, not as an acceptance number.
A common assumption is that Type III is simply a stronger version of Type II. For corrosion, that is not reliably true. In the specification, Type III coatings are left unsealed when maximum abrasion resistance is the main function, and corrosion testing applies only when sealing is specified. Type II coatings, by contrast, are sealed by default unless the order says otherwise.
So a bare hardcoat on an outdoor housing may protect less than a sealed Type II coating, because the sealing step is what closes the pores. If a part needs both wear and corrosion resistance, specify the sealing requirement explicitly and expect some loss of abrasion resistance.
Type II is the practical route for dyed color; the specification itself prefers it for parts that will be dyed. Type III is typically limited to natural gray through black. Whichever type is used, Nova’s guide to surface finishes for custom parts cautions against treating dyed anodizing as an exact Pantone or RAL match and recommends approving a physical sample for color-sensitive work.
Anodizing converts the aluminum surface into oxide, so the coating grows inward and outward. The specification’s design guidance states that dimensions increase by about one half of the coating thickness on each coated surface. A diameter measured across two coated faces therefore changes by roughly one full coating thickness: a shaft grows and a bore shrinks.
The arithmetic below follows that guidance and the specification’s thread rule, under which the pitch diameter of a 60° thread increases by four times the surface growth. It is a starting allowance, not a process capability. Saola Manufacturing’s dimensional-change guide uses the same rules to build pre-anodize allowances.
| Coating thickness | Growth per surface | Diameter change (shaft up, bore down) | Pitch-diameter change, unmasked 60° thread |
|---|---|---|---|
| Type II, 0.0005 in (about 13 µm) | 0.00025 in (about 6 µm) | 0.0005 in (about 13 µm) | +0.0010 in (about 25 µm) |
| Type III, 0.002 in (about 51 µm) | 0.001 in (about 25 µm) | 0.002 in (about 51 µm) | +0.004 in (about 102 µm) |
| Type III, 0.003 in (about 76 µm) | 0.0015 in (about 38 µm) | 0.003 in (about 76 µm) | +0.006 in (about 152 µm) |
Processors sometimes work from their own empirical growth ratios for thin Type II coatings. Ask the finisher for its measured data rather than relying on a single rule.

Consider an illustrative example, not a customer case. A 20 mm bore must finish between 20.000 and 20.021 mm after Type III hardcoat at the default 0.002 in (about 51 µm) nominal. The specification allows that coating to vary by ±20%, so the coating could be anywhere from about 41 to 61 µm. Because the bore diameter shrinks by the full coating thickness, the coating variation alone moves the bore by about 20 µm. That consumes nearly the entire 21 µm tolerance before any machining variation is counted.
In a case like that, pre-compensating the machined size will not solve the problem. The realistic options are:
The same logic applies to features such as hole patterns, slots, and bearing seats. Small and tapped holes are a special case: the specification warns that coating thickness inside them can range from no film to a full coating.
Unmasked threads are a frequent trouble spot. A 0.002 in hardcoat adds about 0.004 in to the pitch diameter of a 60° thread, which can exceed the pitch-diameter tolerance of a standard thread class. Threads, dowel holes, and bearing bores are usually masked or finished after anodizing.
Press fits need extra care. The specification states that anodic coatings are brittle and may crack or spall under force fitting. If a design combines an interference fit with an anodized surface, read our guide on CNC press fit tolerances for pins, shafts, and bores. Then decide whether the fit surface should be masked, finished before anodizing, or sized after coating. Drawings should also state whether tolerances apply before or after finishing. Nova’s manufacturing standards for tolerances and inspection note that a released drawing or approved quotation takes precedence over general reference values.
Type III is not suitable for every aluminum alloy. Unless the order says otherwise, the specification excludes alloys with nominal copper above 5.0% or silicon above 8.0%. It also notes that a 0.002 in or thicker hardcoat is very difficult to obtain on high-silicon die castings such as 360, 380, and 383. Heat-treatable alloys should be in a heat-treated temper before anodizing.
For machined parts, aluminum alloy options for CNC parts such as 6061 are often chosen partly for their anodizing response, while 2024 normally needs protective finishing in corrosive environments, according to Nova’s alloy page. If a cosmetic match across several parts matters, specify one alloy and one stock source. Different alloys and lots can anodize to different shades.
Anodic coatings develop voids at sharp corners and edges, and the specification recommends radiusing edges and inside corners before anodizing. This matters for pocketed housings and plates produced through CNC milling of prismatic aluminum parts, where sharp internal corners and thin knife edges are common. Raise any such features during design review, not after the first batch is rejected.
The specification states that anodic coatings can severely reduce the fatigue properties of aluminum alloys, and that thicker coatings generally reduce them more. Cyclically loaded brackets, arms, and fasteners deserve an engineering check before a heavy hardcoat is applied.
The same specification adds that Type III abrasion resistance declines as thickness approaches 0.003 in, and generally does not improve with added thickness. More coating is not automatically more protection. A moderate thickness chosen for the wear duty is usually the better specification than the thickest the anodizer can run.
Some aerospace and defense drawings call out other anodizing specifications. Suppliers may also work to different revisions of MIL-A-8625 or MIL-PRF-8625, so name the governing document and revision on the drawing.

An accurate quote for anodized aluminum CNC components starts with a complete finish callout. Nova’s finishes guidance says to state the finish type, class, standard, thickness, color, cosmetic zones, masked areas, and inspection criteria. Before sending files to a supplier offering CNC machining services, prepare:
Type III usually costs more than Type II per part. That is a reasonable expectation given the thicker coating, tighter thickness control, and frequent masking, but actual pricing depends on part size, racking, and volume and should be quoted rather than assumed.
Nova’s general CNC reference is ±0.005 in (±0.127 mm), with ±0.001 in available on drawing-specified features. Tighter tolerances on an anodized feature should be reviewed with the supplier before the drawing is released.
Type II is a thinner conventional coating for corrosion resistance, appearance, and dyeing. Type III is a thicker, denser hardcoat chosen mainly for abrasion and wear resistance. Type III changes dimensions more and is generally limited to darker colors.
Not automatically. Type III is typically left unsealed when maximum wear resistance is the goal, and corrosion testing applies only if sealing is specified. A sealed Type II coating can protect better in some environments, so state sealing requirements explicitly.
By specification design guidance, each coated surface grows by about half the coating thickness. A 0.002 in hardcoat changes a diameter by about 0.002 in, and raises the pitch diameter of an unmasked 60° thread by about 0.004 in.
They can, but they usually should be masked or controlled separately. Coating thickness varies inside small and tapped holes, and anodic coatings are brittle under force fitting. Mark these features on the drawing and state whether tolerances apply before or after finishing.
Wrought alloys such as 6061 are commonly hardcoated. The specification excludes alloys above 5.0% copper or 8.0% silicon unless approved, and a 0.002 in hardcoat is very difficult on high-silicon die castings. Confirm the exact alloy and temper with the anodizer.