Before You Go, Let’s Talk About Your Parts
Tell us about your part, quantity, and key requirements. Nova Precision Manufacturing Co.,Ltd can help you choose suitable materials and manufacturing processes for your project.

Parting burrs on turned pins start at cutoff. Learn which process, drawing and deburring choices control burr height, edge condition and press-fit risk.
A parting burr is the raised edge, nub or pip left where a cutoff tool separates a turned pin from its bar. On a pin that must enter a bore, seat against a shoulder or carry an electrical or sealing contact, that small feature can cause scored bores, uneven seating, loose particles and rejected lots, even when every diameter passes inspection. Parting burrs rarely come from one cause. They come from tool height, feed strategy, workpiece support, material behavior and the way the drawing defines an acceptable edge. This guide explains where the burr forms, which process variables reduce it, when downstream deburring is justified, and what to specify before requesting a quote.
Parting burrs form because the last part of the cut behaves differently from the rest. As a cutoff tool moves toward the axis of a rotating bar, the diameter it is cutting shrinks. The Practical Machinist parting-off primer explains that spindle speed has to climb to hold the same surface speed. At some point the machine reaches its limit, so cutting speed falls near the center. Material that is not cleanly sheared at that moment is pushed, folded or torn instead. The same source lists the burr or pip left at the center of the workpiece as one of the main parting-off challenges. It notes that insert geometry, tool alignment, cutting parameters and machine condition all influence it.
For a pin, three situations are common:
Each type has a different cause and a different fix, so “burr-free” is not a useful instruction on its own.

Burr height is governed mainly by tool centerline, feed in the final stage of the cut, edge sharpness, workpiece support and material. The table below links common symptoms to likely causes and to what a buyer should ask a supplier to verify.
| Variable | What goes wrong | Typical symptom on the pin | What to verify with the supplier |
|---|---|---|---|
| Tool height relative to the spindle axis | Tool set too low or too high | Larger pip, tool deflection, uneven break | How cutoff tool height is set and re-checked after tool changes |
| Feed in the last portion of the cut | Constant feed through the center | Torn center, nub, tool breakage | Whether feed is reduced near the axis in the program |
| Cutoff tool geometry and wear | Dull or unsuitable edge | Rolled exit burr, smeared end face | Tool life limits, insert grade and replacement interval |
| Workpiece support during separation | Part flexes or drops uncontrolled | Variable nub height, dings on the end face | Whether a sub-spindle or catcher handles the part |
| Material behavior | Ductile or work-hardening alloy | Tenacious burr that bends rather than breaks | Material grade, condition and past burr results on similar alloys |
| Edge specification on the drawing | No defined edge condition | Disagreement over acceptable burr | ISO-style edge callout or a stated edge-break size |
Centerline accuracy matters more in parting than in ordinary turning. Sandvik Coromant’s parting-off guidance recommends holding tool center height within ±0.1 mm when parting to center. It says that positioning below center increases the pip and risks breakage. It also recommends reducing feed when blade overhang is large. Those figures describe Sandvik’s recommendations for general bar and tube parting. Treat them as a reference for how sensitive the process is, not as limits for every machine.
The same Sandvik page recommends cutting feed by up to about 75% roughly 2 mm before reaching the center. It also recommends stopping feed about 0.5 mm before center so the part separates. A lower feed at the center reduces cutting force, while higher feed in the periphery keeps productivity and tool life up.
There is an important caveat for small pins. Those distances are written for larger bar. On a 3 mm pin, the full radius is only 1.5 mm, so the absolute numbers cannot be copied. The principle transfers: slow down and reduce force as the web thins. The actual values must be set and validated by the shop for that diameter, material and tool.
How the pin leaves the bar changes the nub. Sandvik notes that a sub-spindle can pull the part off, which reduces the toughness demands on the tool. It describes stopping feed about 1 mm before center and letting the sub-spindle complete the separation. On Swiss-type turning machines, the sub-spindle can also take the part for back-end work. That opens a second option: leave a controlled nub, then remove it with a facing or chamfering pass in the same cycle. The Practical Machinist primer adds that the process should be planned so the pip stays on the rough stock side rather than on the finished component. That is the reason to ask where the nub will be left.
Material decides how the final web fractures. Free-machining alloys that form short chips generally break more cleanly. Soft, ductile materials and work-hardening alloys, such as many stainless and copper alloys, tend to smear and fold rather than shear. This is a general machining pattern, not a guarantee. Burr size also depends on lot hardness, tool wear and coolant delivery, so confirm with the supplier’s actual results on the same alloy and diameter. Do not assume that a result on brass carries over to stainless.
Prevention is usually more cost-effective than removal for pins with tight end-face or edge requirements, but removal is still necessary for most precision parts. A stable, low-force cutoff reduces burr height before any secondary operation. That lowers the risk that deburring removes too much material or damages the diameter.
A commonly held view is that a slow feed throughout the entire cut is the safest way to avoid burrs. That is only partly correct. Light feed with a rubbing edge can generate heat and, in work-hardening alloys, harden the surface layer, which can make the final break worse. The better approach is a normal, deliberate feed through the bulk of the cut and a controlled reduction only near the axis, as the Sandvik guidance above suggests.
The opposite assumption is also risky: that the lowest-cost process can rely on tumbling to fix whatever the lathe leaves. Tumbling can bend small burrs over rather than remove them, and it may not reach recessed features. The cost lands later, in inspection, rework or field complaints.

The table below is a qualitative comparison. Suitability depends on pin diameter, material and the required edge condition, so ask the supplier to demonstrate the method on a sample.
| Method | Works best for | Main risk for pins |
|---|---|---|
| In-process chamfer or back-end facing | Controlling the edge at the machine, before a burr is formed or left | Needs a sub-spindle or a second operation; cycle time increases |
| Vibratory or barrel tumbling | Simple geometries and general edge softening | Can bend burrs rather than remove them; part-to-part contact marks on soft or slender pins |
| Abrasive brushing | External edges that are accessible | Uneven edge breaks if fixtures are not controlled |
| Manual deburring under magnification | Low volumes, prototypes, critical edges | Operator variation; slow and costly at volume |
| Thermal or electrochemical processes | Hard-to-reach or recessed features | Setup cost, surface effects and material compatibility must be reviewed |
The drawing should state an edge condition rather than just “deburr.” Without a defined limit, the buyer and supplier can reasonably disagree on what counts as acceptable.
BSI’s overview of ISO 13715 explains that the standard covers the indication and dimensioning of undefined edges on technical drawings. Where a defined edge shape such as a 1 × 45° chamfer is required, the general dimensioning rules of ISO 129-1 apply instead. In practice that gives two clear options:
Do not apply the same requirement to every edge. Edges that touch a seal, a bore entry or a contact face may need a tight limit, while non-functional edges can be looser. Specifying a tight limit everywhere raises inspection effort and cost without improving function.
A parting burr or oversized nub on the leading end of a pin can interfere with assembly. If the pin is intended to enter a bore under interference, the entry end is where scoring, shaved material or misalignment begins. The Nova guide on CNC press fit tolerances for pins, shafts and bores lists lead-in chamfers among the details to settle with diameter limits, surface roughness and assembly direction. A defined lead-in chamfer on the pin end is usually a better control than relying on a burr-free end face.
Deburring and facing can also disturb other characteristics. If removing a nub requires re-gripping the pin in a second operation, the new setup can add axis error. Buyers who specify tight runout or coaxiality should read the guide on controlling concentricity in CNC turned shafts. They should also ask whether the end finishing is done in the same setup or in a secondary one.
Slender pins add another difficulty. Deflection near the cutoff changes how the web breaks and can make burr height inconsistent from part to part. The Swiss turning tolerances guide for slender parts covers how guide bushings, tool pressure, heat and inspection affect realistic precision on those geometries.
Choose the machine route according to pin diameter, length-to-diameter ratio and the end-face requirement. The following is a general guide, not a capability claim for any supplier.
| Pin situation | Likely route | Burr-related consideration |
|---|---|---|
| Short pin, larger diameter, simple ends | Conventional CNC turning services | Centerline and last-stage feed control; sub-spindle optional |
| Long, slender pin with finished back end | Swiss-type with sub-spindle | Back-end facing or chamfering in-cycle; guide bushing supports the cutoff |
| Miniature pin with very small features | Swiss-type or micro machining for miniature components | Burr tendency rises as feature size falls, so inspection is magnified |
| Pin with cross-holes or recessed features | Swiss-type with live tools | Secondary burrs at hole exits may need a separate deburring plan |
Nova’s own service pages indicate that deburring and final inspection are included in their production flow, and the micro machining page lists burr inspection among its checks. Burr limits, methods and sampling for a specific part should still be agreed in writing before production.

A request for quotation that lists only diameter and length leaves the supplier to guess the end condition, and the quote will reflect that guess. Include:
A simple, illustrative scenario shows why this matters. Suppose a buyer orders a stainless pin that will be pressed into a housing, but the drawing says only “break sharp edges.” One supplier tumbles the parts, and another adds a programmed chamfer. The two quotes differ and so do the parts, because the drawing did not define what a good pin end looks like. This is a hypothetical example, not a customer case.
Ask questions that reveal process control rather than only equipment lists:
A supplier who can answer with specifics about tool setup and inspection is more likely to deliver stable results than one that answers only with “we deburr everything.”
Burrs form because the cutting edge loses effective cutting speed near the axis and the last thin web of material tears instead of shearing. Tool height error, high feed at the center, a worn edge, poor support and ductile material all make it worse.
Not always. The aim is to control burr height and location to a defined limit. Tool setup, feed reduction at the center, sub-spindle separation and back-end facing can minimize the burr, but a measured edge requirement is more practical than an absolute zero.
Specify a chamfer or radius where the edge is functional, such as a press-fit lead-in. For non-functional edges, an undefined-edge callout under ISO 13715 can set a permitted size. “Deburr” alone leaves the acceptable result open to interpretation.
Not automatically. Swiss turning supports slender parts near the cutting zone, which reduces deflection, and many machines have a sub-spindle for back-end finishing. Burr results still depend on tool setup, feed strategy, material and the edge specification.
Sometimes, for simple geometry and loose requirements. Tumbling may bend burrs rather than remove them and may not reach recessed features. For tight end-face or edge limits, control the burr at the machine and verify with magnified inspection.
Define the inspection method before production. Magnified visual inspection against a stated edge limit is common, and a first-article approval helps. Because bent-over burrs can look acceptable, ask how the supplier distinguishes them from a clean edge.
Provide the material, functional edge locations, chamfer or edge-state requirements, pin geometry, tolerances, inspection method, packaging needs and quantity. These details let the supplier choose in-cycle edge work or a secondary deburring step rather than guessing.